1.2631 Steel material properties as below:

Chemical composition data of Metal 1.2631 Cold work tool steel-DIN 17350-1980 (EN4957-2001)
CSiMnPSCrMoW
0.450.550.801.000.400.600.030 max0.030 max8.009.001.101.301.101.30

Material equivalent of DIN 1.2631 steel
USAGermanyChinaJapanFranceEnglandItalyPolandCzechiaAustriaSwedenSpain
DIN,WNrGBJISAFNORBSUNIPNCSNONORMSSUNE
1.2631 2310X160CRMOV12

Physical properties of 1.2631 Tool Steel
  • Density: 7.85kg/m3
  • Thermal conductivity:
  • Forging ratio: 5:1 Minimum

Mechanical properties of Alloy Steel 1.2631

Hardness: Annealing  230 HB max, Q+T: 55-58 HRc, different hardness according different Tempering temperature.


Heat treatment of 1.2631 Cold work tool steel
  • Annealing: Annealing temperature/℃: 750~800; After the annealing, degree of hardness ≤HBS: 230
  • Quenching: Hardening temperature/℃:1020~1050, Quenching in oil
  • Tempering: Commonly used drawing temperature/℃: 180~250;  After tempering hardness HRC | 100 ℃ : 58; After tempering hardness HRC | 200 ℃ : 57; After tempering hardness HRC | 300 ℃ : 56 ; After tempering hardness HRC | 400 ℃ : 55
  • Normalizing:at Normalizing temperature, then cool in furnace

 


Forged steel properties of Cold work tool 1.2631 tool steel

For forging  1.2631 steel, Slowly Pre-heat, at  temperature/℃: 1100~850 Forged


Processing of Steel Material 1.2631

Otai Special provide the Grinding, milling , polishing, turning, drilling and others machining service as your required tolerances and size.


Packing of 1.2631 steel

By steel Wire Bundling then put in container, or as customer require packing.


Contact us now!  Free sample waiting for you.

Email: [email protected]

Tel:  +86-769- 23190193

Fax:  +86-769-88705839

Please Register To Contact Supplier Toggar Register Now. If You are Already Registered. Login Now